High temperature effect on the mechanical behavior of steel fiber reinforced self-compacting concrete containing ground pumice powder

Thumbnail
Tarih
2019
Yazar
Karatas, M. and Dener, M. and Benli, A. and Mohabbi, M.
Üst veri
Tüm öğe kaydını göster
Özet
This study reports the results of high temperature effects on the properties of steel fiber reinforced self-compacting concrete (SFRSCC) fabricated by replacing cement with ground pumice powder (GPP) as mineral additive at different substitution rates. The mixtures had the same amounts of steel fiber and the binding material with constant water to binder (w/b) ratio of 0.37. In this context, five SFRSCC series were prepared by replacing Portland cement (PC) with 5, 10, 15, and 20% of GPP including the control mix. Sixty cube samples with a dimension of 150 × 150 × 150 mm were fabricated and exposed to curing aged 3, 7, 28, and 90 days to conduct compressive strength tests and a total of 100 × 100 × 350 mm 18 beam samples cured at 28 days were fabricated to perform the flexural strength tests. Durability tests were performed on the 18 cube samples of 100 × 100 × 100 mm subjected to water curing at 28 days. In addition, the relation between the compressive strength and Ultrasonic Pulse Velocity (UPV) of SFRSCC samples was compared aged 1, 3, 14, and 28 days. Samples of SFRSCC were subjected to the temperatures of 200, 400, 600, and 800°C after being cured at 28 days then cooled to room temperature before conducting tests. The results revealed that the compressive strength of all SFRSCC mixes enhanced at 200°C by 5.34 and 3.55% for control and GPP10 mixes respectively. The strength loss of mixes incorporating GPP is about 60% at 800°C. © 2019 fib. International Federation for Structural Concrete
Bağlantı
https://www.scopus.com/inward/record.uri?eid=2-s2.0-85065827554&doi=10.1002%2fsuco.201900067&partnerID=40&md5=88840c0f27ca33b05463d6e461448ff8
http://acikerisim.bingol.edu.tr/handle/20.500.12898/4060
Koleksiyonlar
  • Scopus İndeksli Yayınlar Koleksiyonu [1357]





Creative Commons License
DSpace@BİNGÖL by Bingöl University Institutional Repository is licensed under a Creative Commons Attribution-NonCommercial-NoDerivs 4.0 Unported License..

DSpace software copyright © 2002-2016  DuraSpace
İletişim | Geri Bildirim
Theme by 
Atmire NV
 

 



| Politika | Rehber | İletişim |

sherpa/romeo

Göz at

Tüm DSpaceBölümler & KoleksiyonlarTarihe GöreYazara GöreBaşlığa GöreKonuya GöreBy TypeBu KoleksiyonTarihe GöreYazara GöreBaşlığa GöreKonuya GöreBy Type

Hesabım

GirişKayıt

DSpace software copyright © 2002-2016  DuraSpace
İletişim | Geri Bildirim
Theme by 
Atmire NV